Item Number: Lib-PNCM622
|
Lib-PNCM622 is the precursor powder of NCMOH622 for High Capacity NCM Cathode Powder at your own composition. There are 200 grams in one bottle Note: You must mix the precursor with LiOH. H2O and calcine the mixed powder at 750- 790oC before use
Specification
|
Package
|
200g/bottle in a vacuumed bag
|
Composition
|
NCMOH622 (Ni:Co:Mn = 6.503 : 1.569: 1.928)
|
Configuration
|
Sphere
|
Particle size distribution
|
D10:4.33 μm D50:9.89 μm D90:18.22 μm
|
Specific surface area
|
4.09 m^2/g
|
Tap Density
|
≥1.64 g/cm^3
|
Water Content
|
wt%<0.36
|
|
|
PPH value
|
~ 8.05
|
|
Main Element
|
Required Content (mol)
|
Ratio (Ni:Co:Mn)
|
|
Li
|
0
|
0
|
|
Ni
|
40.0528
|
6.503
|
|
Co
|
9.6601
|
1.569
|
|
Mn
|
11.8743
|
1.928
|
|
Impurity
|
Required(ppm)
|
Typical(ppm)
|
|
Ca
|
<300
|
18
|
|
Cu
|
<50
|
8
|
|
Fe
|
<100
|
18
|
|
Mg
|
<300
|
19
|
|
Na
|
<500
|
232
|
|
Zn
|
<100
|
102
|
|
SO4
|
<5000
|
3300
|
Note
|
MTI does not manufacture this product, and only sell the small quantity to research for development for new generation battery. If you need a larger quantity or have a question for IP, we will forward your inquiry to the producer.
|
Application Notes:
- Please click to see Procedure for Preparing Anode & Cathode Electrode Slurry.
- Please keep the powder in a vacuum box to avoid moisture.
- Please bake the powder in a vacuum oven at 120 - 150 °C before making slurry and coating to ensure max. capacity.
Related Products
|
|
Sale Price: Starting at USD$3,998.00
|
|
Sale Price: Starting at USD$5,998.00
|
Sale Price: Starting at USD$369.00
|
|
| | |
|
| | |
|
Your cart is empty.
Please clear the browsing history before ordering the product. Otherwise, availability and price are not guaranteed. | |
| | |
|
MTI sponsorships: MTI Sponsors Thermoelectrics Workshop
MTI-UCSD Battery Fabrication Lab
MTI Sponsors the Postdoctoral Awards
Upcoming Shows:
|
|