Crystal

 Structure /Lattice Constant(A)

MP oC

Density, g/cm3

Growth Tech

 DyScO3

 Orthorombic   a=5.44  b=5.71  c=7.89

 2127

 6.9

 CZ

 GdScO3

 Orthorombic  a=5.45  b=5.75  c=7.93

 2127

 6.6

 CZ

TbScO3

Orthorhombic, a = 5.4543, b = 5.7233  c = 7.9147

2127

 6.6

CZ

  • U.S. Dept. of Commerce requires End User Certificate for exporting this product. For certain oversea customer, we may request you to fill the form of STATEMENT BY ULTIMATE CONSIGNEE AND PURCHASER
  • Warning:  The above single crystals are extremely difficult grown due to the ultra-high melting point.  Nobody can promise each substrate has no defect such as domain, dislocation, and twins  If your application is very sensitive to the defects,  you must check substrate by XRD before growing film.  MTI will replace the unsatisfied substrate which has no film grown and no damaged at free of charge until you are satisfied.   No order cancelation is accepted.

Shopping Cart
Your cart is empty.
Please clear the browsing history before ordering the product. Otherwise, availability and price are not guaranteed.
Mailing Lists
MTI sponsorships:
MTI Sponsors Thermoelectrics Workshop

MTI-UCSD Battery Fabrication Lab


MTI Sponsors the Postdoctoral Awards

Upcoming Shows:
2019 MRS Spring April 22 - 26 Phoenix AZ Booth 501

AABC 2019 Jun 24-27 San Diego CA Booth 32

ICT/ACT 2019 Jun 30 - July 4 Gyeongju South Korea

Recent Attended Shows:
36th International Annual Battery Seminar & Exhibit Mar 25-28 Fort Lauderdale FL

TMS 2019 March 10-14 San Antonio TX


APS March Meeting 2019 March 4-8 Boston MA


Click here to see our past conferences

 

Notices
1. Prices listed online are valid for US market and whom pay by credit card only. There will be extra charges for shipping & handling. Price various from country to country.
2. We may add extra charges for paper order and net30 terms due to extra labor cost.
3. The prices listed are subject to change without notice.