Ni-based superalloy tube vessel (30mm O.D x 12 mm I.D x 580 mm L). It can be used under ultra-highly oxidizing and inert gas atmosphere up to 1100°C to process special compounds. It is consumable part of OTF-1200X-HP-30A which is a compact HIP (hot isostatic pressure) furnace for researching the new generation of materials at low cost.

Specification:
    Outside Diameter:          30 mm
    Inside Diameter:           12 mm
    Tube Length:                             580 mm
    Weight:          9.35 lb
    Max. working temperature
    without load:  
         1100 °C
     Working Pressure
             &
    Temperature:
 
Maximum pressure inside the tube
Heating temperature
Max. 2900 PSI  (20 Mpa) 800°C
Max. 1740 PSI  (12Mpa) 900°C
Max. 870 PSI   (6 Mpa) 1000°C
Max. 580 PSI   (4 Mpa) 1100°C
Warning
  • Please set up pressure alarm point in digital pressure display before operation
  • Must install a pressure regulator on gas cylinder to increase pressure gradually.
  • Service life depends on the maximum operation temperature and sample used. The high-pressure vessel is a consumable part, please order replacement once observed deformation.
Standard package
 Name
QTY
Ni-based superalloy tube vessel) 1 set
Flange  1 set
Bolts  1 set
Copper Ring 1 set
Optional Accessories                             
      Installation:
      Attention:
  • In order get longer tube service life, Please use quartz or alumina crucible to carry the sample, instead of loading sample directly inside the tube, please click the picture below to choose one crucible boat:
                                       

Related Products

Shopping Cart
Your cart is empty.
Please clear the browsing history before ordering the product. Otherwise, availability and price are not guaranteed.
Mailing Lists
MTI sponsorships:
MTI Sponsors Thermoelectrics Workshop

MTI-UCSD Battery Fabrication Lab


MTI Sponsors the Postdoctoral Awards

Upcoming Shows:
APS March Meeting 2019 March 4-8 Boston MA Booth 312

TMS 2019 March 10-14 San Antonio TX Booth 101

36th International Annual Battery Seminar & Exhibit Mar 25-28 Fort Lauderdale FL Booth 121

Recent Attended Shows:
2018 MRS Fall Meeting Nov 26-29 Boston MA

MS&T 2018 Oct 14-18 Columbus OH


Furnaces North America Oct 8-10 Indianapolis IN


Click here to see our past conferences

 

Notices
1. Prices listed online are valid for US market and whom pay by credit card only. There will be extra charges for shipping & handling. Price various from country to country.
2. We may add extra charges for paper order and net30 terms due to extra labor cost.
3. The prices listed are subject to change without notice.